# How to Prepare Wood for Painting: Bare Wood and Painted Wood

Source: https://burnandgrain.com/blog/how-to-prepare-wood-for-painting
Published: 2026-10-27
Publisher: Burn and Grain

To prepare bare wood for painting, sand it smooth with 120 then 180 or 220 grit, remove all dust, and apply a primer or sealer so the paint does not soak in unevenly. Wood that is already painted needs a different approach: clean it, scuff the glossy surface with fine sandpaper, fill any damage, and prime with a bonding primer before the new coat. The steps below cover both cases, with the grits and drying times that matter for small craft pieces such as plaques, signs and wood blanks.

## Start with the surface type

The right preparation depends on what is on the wood now. Bare, unfinished wood is porous and drinks paint unevenly, so it needs sanding and a primer or sealer. Wood with an old paint film needs cleaning and scuffing so the new coat can grip. Wood with a clear varnish, wax or oil needs the finish removed or at least dulled, because paint does not bond to a slick surface.

A quick test tells you which you have. Put a drop of water on the surface. If it soaks in within a minute or two, the wood is bare. If it beads up, there is a finish or paint that needs scuffing or stripping first.

## Sand in stages and remove the dust

For bare wood, start at 120 grit to level rough spots, then finish at 180 or 220 grit. Going finer than 220 can burnish the surface so paint and stain soak in less. Sand with the grain, never across it, because cross-grain scratches show through paint, especially in thin coats.

After sanding, remove every trace of dust. Vacuum or brush it off, then wipe with a lightly damp cloth or tack cloth and let the wood dry. Dust left on the board turns into bumps under the paint and prevents a clean line with markers or fine brushes. Small craft blanks, such as plaques and rounds, are often already sanded smooth, and a quick pass with 220 grit is enough.

[See smooth wood blanks](https://burnandgrain.com/best/best-wood-blanks-for-pyrography)

## Seal knots and soft spots, then prime

Pine and other resinous woods can bleed sap or tannin through paint, leaving yellow or brown stains, mainly around knots. Dab a shellac-based primer or knot sealer over knots before the full primer coat. On large flat areas, one coat of primer evens out how much paint the wood absorbs, so the finish color looks the same across the board.

Choose the primer by the paint. A water-based primer works under acrylic and latex paint, and shellac or oil-based primer blocks stains better. Let it dry fully, then sand lightly with 220 grit to knock down raised grain and wipe off the dust again. For small pieces painted with acrylic paint pens, a thin coat of clear water-based sealer or gesso can take the place of a primer.

## Preparing wood that is already painted

Wash the surface with warm water and mild detergent to remove grease and dirt, then rinse and dry it. If the paint is flaking, scrape off loose areas and feather the edges with 120 grit so the repair does not show as a ridge. Fill dents or gouges with wood filler, let it dry, and sand it flush.

Then scuff the whole surface with 180 to 220 grit until the shine is gone. You do not need to remove sound paint, only dull it. Wipe off the dust and apply a bonding primer, which is made to stick to glossy surfaces. Skip this and the new paint can peel in sheets. Old paint from before the late 1970s may contain lead, so test it with a kit before sanding, and do not dry sand it if it tests positive.

## Wood you plan to burn first

If the project includes pyrography, burn before painting. Heat on painted or primed wood produces fumes and does not give a clean dark line, and paint scorches. Sand the bare wood, burn the design, then brush off ash and add color on top. Our article on wood burning over finished or painted wood explains why. Colors go on afterward with pencils, watercolor, acrylic or paint markers, each compared in the paint guide. Seal the project once the color is dry so the paint and burn marks are protected.

[Compare pyrography paints](https://burnandgrain.com/best/best-paint-for-pyrography)

## Painting and drying tips

Apply thin coats, not one thick coat. Two or three thin coats dry harder and show fewer brush marks. Let each coat dry to the touch, and check the label for recoat times, which for water-based acrylic is often under an hour but longer in cool or humid rooms. Paint markers also lay down better on a primed or sealed surface than on raw wood, which pulls color unevenly.

For small craft work, paint markers give clean edges without a brush. Fine and medium tips are the most useful sizes on wood, and the Posca marker guide compares sets by tip. Let paint cure for a few days before heavy handling, even if it feels dry in an hour.

[Compare Posca paint markers](https://burnandgrain.com/best/best-posca-paint-markers)

## Frequently asked questions

Do I need to sand painted wood before repainting? Usually yes. Scuff sanding with 180 to 220 grit dulls the gloss so primer and paint grip. Only chalky, matte paint in good condition may need only cleaning.

Do I have to prime bare wood? For anything beyond a quick craft piece, yes. Primer evens out absorption and blocks stains. Some paint-and-primer products reduce the work, but resinous woods and knots still benefit from a sealer.

What grit should I stop at before painting? 180 to 220 grit. Coarser leaves scratches that show through, and much finer can leave the surface too smooth for good adhesion.

Can I paint over varnished wood? Yes, if you sand the varnish dull and use a bonding primer. Painting over a glossy, untouched varnish will usually peel.

## Gear guides for this topic

- https://burnandgrain.com/best/best-posca-paint-markers
- https://burnandgrain.com/best/best-paint-for-pyrography
- https://burnandgrain.com/best/best-wood-blanks-for-pyrography